Towers and chimneys in an industrial plant area rise in groups under sunlight
After the ink and resin vehicle undergo high-shear dispersion, microbubbles remain trapped inside the ink layer and are slow to disappear; pinholes and craters surface first on the drawdown sheet, blank dots then appear on the printed colour blocks, and ink adjustment and regrinding pin the shift's output down at the dispersion step.
Chemi Tech supplies the KM-702 series of defoamers for the microbubble problem in oil-based ink and resin vehicle systems; the dosage is adjusted flexibly by vehicle viscosity, dispersion line speed and resin polarity. This grade is a mineral-oil type; coexisting with common resins and solvents, it neither separates nor turns cloudy, and it causes no interference with the gloss and fineness of the ink layer. The measured data on pinhole density and ink-layer gloss are recorded side by side at the same dispersion batch, and the fitted dosage of the KM-702 series is determined accordingly; resin polarity and solvent ratio are checked together before the dosage of that ink batch is set.
Advantages of Chemi Tech Defoamers
The Chemi Tech KM-702 series defoamer is configured for oil-based ink and resin vehicle systems. It is a mineral-oil type; coexisting with resins and solvents, it neither separates nor turns cloudy; its compatibility is excellent, so the gloss and fineness of the ink layer do not drop due to dosing; it breaks foam fast, clearing the microbubbles after high-shear dispersion within the settling section; its foam-suppressing duration is long-lasting, so no shift-by-shift top-up is needed in the ink tank; it causes no interference with pigment wetting, keeping the colour strength reading of the colour blocks stable; and the dosage is economical, rated by vehicle viscosity and line speed, so the additive cost per tonne of ink can be accounted directly.
Industry Pain Points and Solutions
The root of microbubbles in oil-based systems lies mostly in the combined effect of a too-high vehicle viscosity and air entrained by high-shear dispersion, while differences in resin polarity stabilise the microbubbles inside the ink layer, finally concentrating in two places: pinhole density and gloss reading.
When the vehicle viscosity rises, the microbubbles after dispersion are retained by the ink layer and pinholes show first on the drawdown sheet. KM-702 has excellent compatibility; once the two readings of viscosity and line speed are cleared, its dosage is re-rated by the polarity of that ink batch, and the pinhole density falls accordingly.
After the resin polarity is switched, the same dosage performs differently across two vehicle batches and the gloss reading differs markedly; with an alkyd vehicle and an acrylic vehicle compared side by side, the drop in gloss from fifty-eight to fifty-two narrows to within two divisions, and the dosage is rated to the fitted grade of that batch.
As the standing time in the ink tank lengthens, microbubble regeneration consumes the foam-suppressing margin. The KM-702 series adds no extra top-up frequency on this item; once viscosity, polarity and line speed are all checked through, the fitted dosage of that ink batch is settled and the ink-adjustment shift continues at that grade.
Typical Operating Conditions and Verification
Customer case: the resin-vehicle dispersion workshop of an ink manufacturing enterprise in Guangdong, applied to the grinding and ink-adjustment stages of oil-based inks.
At this plant the pinhole density of two resin-vehicle batches differed markedly, craters on the drawdown sheet were denser on the acrylic batch, and the gloss reading was lower on the alkyd batch. KM-702 was selected as the defoaming grade for that ink batch after comparison, with the dosage rated by vehicle viscosity and dispersion line speed. Reading changes after commissioning: the pinhole density of the two ink batches converged; craters on the drawdown sheet basically no longer appeared; the gloss reading between the two batches narrowed to within two divisions; and the top-up frequency in the ink tank fell from once per shift to once per day.
Frequently Asked Questions
If the KM-702 series is used continuously in an oil-based vehicle system, will it pull the gloss and fineness of the ink layer off target?
The two clues of resin polarity and solvent ratio must be sorted out to judge whether the pinholes and craters fall within the assessed range of that ink batch. The KM-702 series coexists with common resins and solvents without separating or turning cloudy; the measured data on pinhole density, gloss reading and fineness are given side by side by Chemi Tech after comparing the two vehicle batches, and dosing at the rated magnitude does not disturb the colour strength reading of the colour blocks. The actual dosage is further corrected by the vehicle viscosity of the current batch; Chemi Tech derives the fitted dosage from the comparison results of the two ink batches.