Multi-coloured fibre materials spread out in horizontal layers

After the water-repellent finishing of polyester curtain fabric, the spray rating drops notch by notch through several rounds of washing; water droplets spread on the fabric surface instead of rolling off, wet spots appear first at the turned edges and folds, and re-finishing batches pin the finishing workshop's schedule down at the water-repellency step.

Chemi Tech supplies the KMF-2802 series of water repellents for the water-repellent finishing of polyester curtain fabric; the dosage is adjusted flexibly by fabric weight, wet pick-up and curing temperature. This grade forms a continuous film on the fibre surface, balancing spray rating with hand feel, and is compatible in the same bath with common softeners and resin finishing agents, keeping the perfluorinated item within the detection limit. The measured data of the AATCC 22 spray rating and the number of wash-fastness cycles are laid on the same finishing record, and the fitted dosage of the KMF-2802 series is graded accordingly; the finishing dosage is set only after fabric weight and curing conditions are checked through.

Advantages of Chemi Tech Water Repellents

The Chemi Tech KMF-2802 series water repellent is configured for the water-repellent finishing of polyester curtain fabric. It forms a continuous film on the fibre surface, keeping the spray rating in the pass grade; it is wash-fast, so rating decay slows after multiple rounds of washing; it has little effect on hand feel, leaving the polyester fabric neither stiff nor harsh; its compatibility in the same bath with common softeners and resin finishing agents is excellent, so the finishing bath needs no separate formulation; its curing-temperature window is wide, so the fabric mill's existing curing conditions can be carried over directly; and it follows a fluorine-free route, keeping the perfluorinated item within the detection limit and covering the compliance items of export orders.

Industry Pain Points and Solutions

The root of water-repellency decay on polyester curtains lies mostly in the combined effect of a too-low wet pick-up and insufficient curing crosslinking, while the low surface energy of polyester fibres weakens the continuity of the finishing film round by round, finally concentrating in two places: the spray rating and the appearance of wet spots.

When the wet pick-up is too low, the film formed on the fibre surface is not continuous enough and the spray rating drops one notch after the first few rounds of washing. KMF-2802 forms a continuous film; once the wet pick-up and curing temperature are checked through, its dosage is re-rated by the fabric type and the spray rating stays in the pass grade.

When the curing temperature is set too low, crosslinking is insufficient, the spray rating falls with each round of washing and spreading wet spots remain on the face of the turned edge. KMF-2802 performs stably across dyed and greige grades; with curing at one hundred and twenty degrees Celsius and one hundred and fifty degrees Celsius compared side by side, rating decay narrows from three notches to one, and the finishing-bath concentration is graded accordingly.

Mechanical friction during washing puts the finishing film through another test. The KMF-2802 series is wash-fast and adds no extra re-finishing rounds on this item; once fabric weight, wet pick-up and curing temperature are all checked through, the fitted dosage of this batch of fabric is settled and the finishing workshop continues to use that grade.

Typical Operating Conditions and Verification

Customer case: the water-repellent-finishing workshop of a curtain-fabric finishing enterprise in Fujian, applied to the curing-finishing stage of polyester curtain fabric.

At this plant the spray rating of the dyed batches fell faster after washing than that of the greige batches, the spread of wet spots at the turned edges was wider than on the body of the fabric, and re-finishing rounds rose month by month. Based on comparison of fabric weight and washing conditions, KMF-2802 was adopted as the finishing grade for that batch of fabric; the finishing-bath concentration was rated by wet pick-up and curing temperature. Measured records after finishing: the rating decay of the dyed batches converged with that of the greige batches; wet spots at the turned edges no longer spread to the back of the fabric; the spray rating stayed in the pass grade after multiple rounds of washing; re-finishing rounds decreased, and the finishing schedule was completed to plan.

Frequently Asked Questions

In fluorine-free finishing of polyester, can the decay of the spray rating after multiple rounds of washing be predicted?

The three readings of fabric weight, wet pick-up and curing temperature must be compared together. The KMF-2802 series forms a continuous film on the fibre surface and is wash-fast; the measured data of the spray rating and wet-spot rating are checked out by Chemi Tech from the washing records of the same fabric type, the decay trend can be plotted as a curve against the number of rounds, and the specific values are subject to the actual conditions of that finishing mill. The actual dosage is fine-tuned by wet pick-up and curing temperature; Chemi Tech determines the fitted dosage by combining lab samples with production-line measurements.