A tall red-and-white striped chimney rising vertically against a blue sky
After the dry-mix mortar tumbles at high speed in the mixer, flocs are hard to break up, the tank-mouth foam persists, the discharge fluidity differs markedly between two batches, and the contractor pins re-mixing and material top-up down at the mixing step.
Chemi Tech supplies the KM-9255 series of defoamers for the mixing stage of cement-based dry-mix mortar; the dosage is adjusted flexibly by the powder moisture content, mixing speed and water-addition ratio. This grade is a nano-polymer type, with high compatibility, resistance to corrosion, high temperature, acid and alkali, and it separates out in neither the dry-blending nor the water-mixing stage, causing no interference with the setting time of the mortar. The measured data on discharge fluidity and tank-mouth foam-layer height are recorded side by side at the same mixing batch, and the fitted dosage of the KM-9255 series is determined accordingly; the dosage is given only after the powder moisture content and mixing tempo are checked together.
Advantages of Chemi Tech Defoamers
The Chemi Tech KM-9255 series defoamer is configured for the mixing stage of cement-based dry-mix mortar. It is a nano-polymer type with high compatibility, competing for no water with the cementitious material; it breaks foam fast, so the tank-mouth foam layer falls back within a short time after water is added and mixed; its foam-suppressing duration is long-lasting, so no batch-by-batch top-up is needed during discharge standing; it resists acid and alkali, so its foam-suppressing ability does not decay as powder alkalinity rises; its viscosity reduction is marked, so the discharge fluidity converges between two batches; and the additive cost per tonne of mortar can be read directly from the batching sheet.
Industry Pain Points and Solutions
The root of foaming in cement-based dry-mix mortar lies mostly in the combined effect of a too-high powder moisture content and air entrained by mixing shear, while fluctuations in the water-addition ratio stabilise the fine bubbles inside the slurry, finally concentrating in two places: fluidity loss and the tank-mouth foam layer.
When the water addition is one grade lower, powder flocs first show at the tank mouth and the discharge fluidity drops faster than the nominal value. KM-9255 has high compatibility; once the two readings of moisture content and mixing speed are cleared, its dosage is re-rated by the mix ratio of that mortar batch, and the fluidity loss narrows accordingly.
After the mixing speed is raised, the same dosage performs markedly differently at the low-speed and high-speed grades, and the tank-mouth foam-layer height is higher at the high-speed grade. KM-9255 is compared side by side at low and high mixing speeds; the foam-layer height drops from twelve centimetres to four centimetres, and the dosage is rated to the fitted grade of that line.
When the dry powder cakes from moisture, the stable period of the fine bubbles is further extended and the foam-suppressing margin is consumed step by step. KM-9255 adds no extra re-mixing passes on this item; once moisture content, mixing speed and water-addition ratio are all checked through, the fitted dosage of that line is made clear and the mixing stage accounts for water addition and additive side by side.
Typical Operating Conditions and Verification
Customer case: the ready-mixed mixing workshop of a dry-mix mortar producer in Shandong, applied to the mixing and discharge stage of cement-based dry-mix mortar.
At this plant the fluidity loss of two mortar batches differed markedly, the tank-mouth foam layer was thicker on the moisture-affected batch, and re-mixing passes rose month by month. KM-9255 was selected for the plant as the defoaming grade for that line, with the dosage rated by powder moisture content and mixing speed. Reading changes after commissioning: the fluidity loss of the two batches converged; the tank-mouth foam layer fell within the observation mark; re-mixing passes fell from three per shift to once per day; and the contractor's material top-up sheet no longer had batch-by-batch additions.
Frequently Asked Questions
If the KM-9255 series is dosed over the long term in dry-mix mortar, will it affect the discharge fluidity and setting time?
The three items of water addition, mixing speed and powder moisture must be checked together. The KM-9255 series is a nano-polymer type with high compatibility and acid-alkali resistance; the measured data on discharge fluidity and tank-mouth foam-layer height are given side by side by Chemi Tech at two mixing-speed grades, and dosing at the rated magnitude does not disturb the setting time of the mortar. The actual dosage is corrected by the discharge fluidity; Chemi Tech derives the fitted dosage from the two readings at the mixing stage.