An aerial view of a refinery, with densely arranged fractionation towers, storage tanks and piping
In the interval between drum switches, the level-gauge needle at the coke-drum top rises to the upper limit again, coke-powder entrainment at the fractionator bottom increases accordingly, and unit throughput is pushed down by one notch.
Chemi Tech supplies the KM-6100 series defoamer for delayed coking units at refineries. It withstands high temperature and both acid and alkali, can be shared between the coke drum and the amine regeneration system, and does not interfere with the separation of coker distillate. The dosage can be adjusted flexibly according to top temperature, switching cycle and amine circulation rate; what holds it together under the high temperature inside the tower is a formulation matter and will not be expanded here. For units that likewise see a falsely high level after a coke-drum switch, the two readings of top temperature and coke-powder entrainment can be compared first.
Advantages of Chemi Tech Defoamers
The Chemi Tech KM-6100 series defoamer is designed for the delayed coking section at refineries. It withstands high temperature, keeping foam-breaking speed stable as the top temperature rises; it withstands acid and alkali, so alkalinity swings in the amine regeneration system do not cause separation or oil floating; its compatibility is excellent, with no precipitation alongside distillate; its foam-suppressing effect is long-lasting, so the foam layer thins markedly in the interval between switches; and its dosage is economical, rated by top temperature and switching cycle, with the chemical cost at each temperature grade clear in the records.
Industry Pain Points and Solutions
A falsely high level at the coke-drum top usually stems from the combined effect of a rising top temperature and a shortened switching cycle; coke powder is carried by foam into the fractionator, and bottom fouling plus throughput loss are the two items that surface last.
Before and after a coke-drum switch, the foam layer at the top thickens first and the level gauge diverges from on-site sampling. KM-6100 withstands high temperature; the two readings of top temperature and switching cycle are worth laying out side by side, the dosage is rated separately against the load of that unit, and the gauge deviation narrows markedly.
When the temperature difference in the amine regeneration system widens, the same dosage breaks foam at noticeably different speeds across two temperature grades. Comparing the low and high grades side by side, the top foam-layer height falls from forty centimetres to twelve centimetres, and the dosage is recorded separately by temperature grade.
As throughput is raised, the vapour and liquid load in the tower rises with it and the stable period of the foam lengthens. The KM-6100 series has a long-lasting foam-suppressing effect, so skimming and tower-cleaning frequencies need not be added; the dosage must follow throughput, however, recorded separately for the high and low grades, and the readings are worth checking once more before the next switch.
Typical Operating Conditions and Verification
Customer case: the delayed coking workshop of a refinery in Shandong, applied to the defoaming stage at the coke-drum top and in the amine regeneration system.
They worked it back from throughput: in those months the unit load was cut by one notch, the top level gauge alarmed frequently, and coke-powder samples at the fractionator bottom were consistently high. Tracing two months back, the foam layer in the interval between switches had already covered half of the sight glass. After comparing the two grades of top temperature and switching cycle, KM-6100 was chosen as the defoaming grade for this unit, with the dosage rated by amine circulation rate and throughput. After commissioning, the top foam layer thinned markedly, level alarms decreased, coke-powder entrainment fell back, and throughput returned to the planned level.
Frequently Asked Questions
With a falsely high top level, should the defoamer be checked first or the switching rhythm?
The two clues of top temperature and switching cycle have to be reconciled together; on a unit where both are at play, adjusting the switching rhythm alone usually cannot bring the level back. The KM-6100 series withstands high temperature and both acid and alkali; the measured data on foam-layer height and coke-powder entrainment are provided by Chemi Tech for two temperature grades of the same unit, and dosing at the rated level does not interfere with distillate separation; the amine circulation rate is the correction item for the actual dosage. Provide the three readings of top temperature, switching cycle and amine circulation rate, and the starting dosage can first be set between the two grades.