An automated production line in a large plant, with an orange overhead crane

Most people attribute the fluctuation of coating basis weight to slurry solid content, yet what really makes pinholes appear on the electrode is often the microfoam that was never brought under control during mixing.

Chemi Tech supplies the KM-1900 series defoamer for battery slurries. It stays alongside the conductive agent and the binder in the slurry without precipitation, and it does not interfere with the basis weight or the compaction of the electrode. The dosage can be adjusted flexibly according to slurry viscosity and solid content; why it still holds the microfoam in a high-viscosity system is a formulation matter and will not be expanded here.

Advantages of Chemi Tech Defoamers

The Chemi Tech KM-1900 series defoamer is designed for the mixing and coating sections of battery slurries. It breaks foam fast, clearing the microfoam of high-viscosity slurry within the standing section; its compatibility is excellent, staying unclouded alongside conductive agent and binder; its foam-suppressing effect is long-lasting, so the refill frequency of the slurry tank drops markedly; its stability is strong, narrowing the basis-weight deviation between two batches; and its dosage is economical, rated by viscosity and solid content. The technician's own words were: no pinholes visible on the doctor-blade sample any more.

Industry Pain Points and Solutions

The root of microfoam in battery slurries mostly lies in the combined effect of rising viscosity and an upward solid-content target; gas entrained during mixing cannot be recovered, and electrode pinholes plus basis-weight deviation are the two items that finally land on the coating step.

After the mixing viscosity rises, the microfoam is held back by the slurry and the fineness on the doctor-blade sample rebounds first. KM-1900 has excellent compatibility; the two readings of viscosity and solid content are recorded separately, the dosage is rated anew against that batch's viscosity, and the fineness reading stabilises.

When the solid-content target is raised, the same dosage breaks foam at noticeably different speeds across two solid-content grades. Comparing the low and high grades side by side, the basis-weight deviation narrows from four grams to one gram per square metre, and the KM-1900 dosage lands in the suited grade of that batch.

Once the coating speed is raised, the microfoam enters the die before it can be cleared in the slurry-storage section. The KM-1900 series has a long-lasting foam-suppressing effect, so the refill frequency can stay as it is; the dosage must follow the coating speed, however, recorded separately for two grades, and once the readings of both grades are laid side by side, the dosage comes out.

Typical Operating Conditions and Verification

Customer case: the electrode slurry workshop of a lithium-battery materials enterprise in Guangdong, applied to the mixing and coating sections of cathode and anode slurries.

The basis-weight readings of two batches of slurry at this plant differed markedly: pinholes appeared first at the electrode edge of the high-solid-content batch, while the deviation of the low-solid-content batch concentrated in the middle of the coating width. After comparing the two grades of viscosity and solid content, KM-1900 was chosen as the defoaming grade for this workshop, with the dosage rated by slurry viscosity and the solid-content target.

After commissioning, the fineness readings of the two batches converged, the basis-weight deviation was brought within one gram, pinholes at the electrode edge decreased markedly, and the refill frequency of the slurry tank fell from once per shift to once per day.

Frequently Asked Questions

With basis weight fluctuating, should the coating parameters be adjusted first, or should slurry defoaming be checked first?

It all depends on whether the viscosity and solid content fall within the normal range for that batch of slurry; on a batch where both run high, adjusting the coating parameters alone usually cannot bring it back. The KM-1900 series stays alongside conductive agent and binder without precipitation; the measured data on fineness reading and basis-weight deviation are given by Chemi Tech for the two solid-content grades of the same batch, and the coating speed is the correction item for the actual dosage. It is worth having these two grade records checked together.