Multicoloured powders and brushes laid out flat on a tabletop as seen from above

The fineness reading of the inorganic pigment in the predispersion slurry keeps rebounding after grinding, flooding and floating show up together in the rub-out test, the slurry viscosity pushes the sand-mill current higher, and the same formulation has to be readjusted with every new pigment batch, so the colour-matching delivery schedule is pinned down at the dispersion step.

Chemi Tech supplies the KMK-1003 series of dispersants for inorganic-pigment predispersion slurry systems; the dosage is adjusted flexibly by pigment particle size, surface treatment and target solids content. This grade's anchoring groups grip the pigment surface firmly and do not desorb under high-shear grinding; its viscosity reduction is marked and its adaptability to inorganic pigments is wide. The measured data on slurry fineness readings and rub-out flooding ratings are listed by pigment grade, and the fitted dosage of the KMK-1003 series can be read out grade by grade; the dosage is settled only after the pigment surface treatment and solids target are listed separately.

Advantages of Chemi Tech Dispersants

The Chemi Tech KMK-1003 series dispersant is configured for inorganic-pigment predispersion slurry. Its anchoring groups grip the pigment surface firmly and do not desorb under high-shear grinding; its viscosity reduction is marked and the sand-mill current stays steady and controllable; its adaptability to inorganic and extender pigments is wide, so switching grades needs no overall readjustment; its storage stability is strong, so the predispersion slurry neither coarsens nor floods; its colour strength and colour development are stable, keeping the rub-out flooding rating consistent; and the dosage is adjusted with the pigment grade and target solids content, so the additive cost of the colour centre can be accounted colour system by colour system.

Industry Pain Points and Solutions

The root of flooding and floating in inorganic-pigment predispersion slurry lies mostly in the mismatch between the pigment surface treatment and the dispersant's anchoring groups, while a raised target solids content compresses the distance between particles to a critical value, finally concentrating in two places: fineness rebound and rub-out floating.

When the pigment grade changes, the well-anchored dispersant is thrown off by the polarity of the new surface and the fineness reading rebounds repeatedly around the pass line. KMK-1003 makes anchoring comparisons by pigment grade and surface treatment; once the two clues are cleared, the dosage is rated grade by grade and the fineness reading no longer rebounds.

Once the target solids content is raised, the slurry viscosity pushes the sand-mill current higher, grinding time is forced longer, yet the fineness still cannot be brought down. KMK-1003 reduces viscosity markedly; with the low-solids and high-solids grades compared side by side, the sand-mill current drops from eighteen amperes to twelve amperes, and the dosage is rated to the fitted grade of that colour system.

Coarsening and flooding during storage are also within consideration. The KMK-1003 series is fully anchoring and adds no extra regrinding passes on this item; once the comparisons of grade, surface treatment and solids content are complete, the precise dosage of that colour system is graded and the colour centre doses by it.

Typical Operating Conditions and Verification

Customer case: the inorganic-pigment predispersion workshop of an industrial coating enterprise in Shandong, applied to the grinding and blending stages of multiple pigment grades.

This plant changed three pigment suppliers in the first half of the year; the fineness reading of the same formulation differed markedly across the three grades, and the rub-out flooding rating passed only on one of them. KMK-1003 was matched as the dispersing grade for that centre after comparison of pigment grade and solids target, with the dosage graded by surface treatment. The regrinding records show: the fineness readings of the three grades converged; all flooding ratings fell within the pass range; the sand-mill current no longer fluctuated sharply with the grade; regrinding passes decreased, and the colour-matching delivery schedule was completed to the original plan.

Frequently Asked Questions

Can a single dispersant work across multiple inorganic pigment grades?

It is constrained by two clues: the pigment surface treatment and the target solids content. The KMK-1003 series makes anchoring comparisons by pigment grade and has wide adaptability to inorganic pigments; the measured data on fineness readings and rub-out flooding ratings are given by Chemi Tech from per-pigment comparisons within the same colour system, and colour strength is not weakened within the rated dosage range. The actual dosage takes the pigment grade and target solids content as correction items; Chemi Tech gives the fitted dosage of that colour system from the per-pigment comparison results.