A plasma cutting head striking an arc of sparks on a metal plate
After plastic parts are sprayed with waterborne plastic paint, edge retraction appears on the panel surface first and orange peel then covers the whole painted surface; the interlayer adhesion of the two-pass spray fails the cross-cut test, and rework and touch-up spraying pin the throughput down at the coating step.
Chemi Tech supplies the KMP-1707 series of levelling agents for the leveling of waterborne plastic paint spraying; the dosage is adjusted flexibly by spraying tempo, wet-film thickness and flash-off window. This grade markedly lowers the dynamic surface tension, letting the wet film spread fully within the flash-off window; its compatibility is excellent and causes no craters, while leaving margin for recoatability. The measured data on the orange-peel grade of the panel surface and the cross-cut adhesion grade are filed into the same test-panel record; the fitted dosage of the KMP-1707 series is settled at this grade of the line, and the dosage is adjusted by the measured results of film thickness and flash-off window.
Advantages of Chemi Tech Levelling Agents
The Chemi Tech KMP-1707 series levelling agent is configured for waterborne plastic paint spraying. It lowers surface tension markedly and lets the wet film spread fully within the flash-off window; edge retraction at panel edges basically disappears, with even corner coverage; the orange-peel grade of the panel surface rises and gloss uniformity improves in step; its compatibility is excellent, causing no craters and no effect on interlayer adhesion; it leaves margin for recoatability, keeping the interface of the two-pass spray stable; its thermal stability is strong, with no decomposition or yellowing in the baking section; and the loss from re-spraying and touch-up narrows in step.
Industry Pain Points and Solutions
The root of orange peel on a coating line lies mostly in the combined effect of a too-short flash-off window and a too-steep surface-tension gradient across the wet film, while raising the chain speed further compresses the spreading time, finally concentrating in two places: orange peel on the panel surface and edge retraction at the panel edges.
When the spraying tempo is speeded up, the wet film has no time to spread within the flash-off window and the orange peel sets first. KMP-1707 lowers surface tension markedly; once the spraying tempo and flash-off temperature are set, its dosage is re-rated by the chain speed of that line, and the orange-peel grade of the panel surface rises one notch.
When the wet-film thickness is set higher, the surface-tension gradient at the panel edge amplifies and edge retraction follows. KMP-1707 performs stably across both thick-film and thin-film grades; comparing side by side the orange-peel grades of the panel surface at thick-film and thin-film grades, the gloss uniformity of the thick-film grade after baking approaches that of the thin-film grade, and the film thickness at corners no longer falls noticeably.
When the flash-off window is compressed, the most easily disturbed is the recoat interface. KMP-1707 leaves margin for recoatability and adds no extra sanding step on this item; with tempo, film thickness and flash-off all checked through, the fitted dosage of that line is settled and the coating line locks its dosage within this range.
Typical Operating Conditions and Verification
Customer case: the spraying workshop of a plastic-products enterprise in Zhejiang, applied to the spray-leveling stage of a waterborne plastic paint topcoat.
At this plant edge retraction at the panel edges recurred repeatedly, orange peel was distributed in patches across the same workpiece, and the cross-cut result of the two-pass spray was good on some panels and poor on others. The plant switched to KMP-1707 as the leveling grade for that line, with the dosage rated by spraying tempo and wet-film thickness. Measured performance after the switch: the orange-peel grade of the panel surface rose one notch; edge retraction at the panel edges basically no longer appeared; the cross-cut result of the two-pass spray passed stably; the count of reworked and touch-up parts fell back, and the shift plan was completed to the original schedule.
Frequently Asked Questions
If the dosage of the KMP-1707 series is increased, will it instead cause craters or weaken interlayer adhesion?
The key is whether the wet film spreads sufficiently within the flash-off window. KMP-1707 has excellent compatibility and causes no craters at normal dosage, leaving margin at the recoat interface; the measured data on orange-peel grade and gloss readings are checked out by Chemi Tech from the test-panel records of the same coating line, and within the rated comparison range they do not weaken interlayer adhesion. The actual dosage is re-calibrated by spraying tempo and wet-film thickness; Chemi Tech checks the test-panel results against the production-line measurements and gives the fitted dosage.