Towers and pipe racks of an industrial plant stretching horizontally in the distance

After rosin size is added to the white-water system of a paper machine, a layer of fine, dense foam floats on the surface of the wire-pit white water; the foam returns with the white-water circulation to the spray piping, fish eyes and mottling appear on the paper surface, and the papermaking speed is forced down.

Chemi Tech supplies the KM-902 series of defoamers for surface foam in papermaking white water with rosin size; the dosage is adjusted flexibly by the white-water temperature and the rosin-size dosage. This grade is a silicone-based formulation, designed for production lines where temperature is not the main contradiction and mechanical foam dominates; it breaks foam fast in the white-water circulation system without aggravating fibre flocculation. The measured data on the count of paper-surface mottling and the foam height in the white-water pit are filed into the same papermaking record; the precise dosage of the KM-902 series can be read out grade by grade, and the dosage is rated in grades by the white-water temperature difference and the rosin-size dosage.

Advantages of Chemi Tech Defoamers

The Chemi Tech KM-902 series defoamer is configured for papermaking white-water systems. It breaks foam fast, and the mechanical foam brought by rosin size falls back noticeably in a short time; it is a silicone-based formulation with a strong foam-breaking power against mechanical foam; its compatibility is excellent, coexisting with rosin size and fibres without producing flocculation; its foam-suppressing duration is long-lasting, and the foam layer in the white-water pit does not readily recur; the dosage is economical, with little effect on gloss and paper appearance; and the defoaming cost per tonne of paper can be apportioned to the papermaking section for accounting.

Industry Pain Points and Solutions

The root of foaming in papermaking white water lies mostly in the combined effect of a high rosin-size dosage and stock-pumping shear, while the fine fibres circulating in the white water further stabilise the foam on the surface of the wire pit, finally concentrating in two places: paper-surface mottling and the foam height in the white-water pit.

When the white-water temperature runs high, the foam layer on the wire-pit surface first thickens and paper-surface mottling increases in step. KM-902 breaks foam fast; once the two readings of white-water temperature and rosin-size dosage are set, its dosage is re-rated by the papermaking speed of that machine, and the foam-layer height falls back noticeably.

After the rosin-size dosage is raised, mechanical foam is entrained into the white-water circulation and paper-surface mottling spreads in step. KM-902 has a strong foam-breaking power against mechanical foam; comparing side by side the counts of paper-surface mottling at low and high rosin-size grades, the time for the low grade to fall back within the pass range is markedly shorter than for the high grade, and the foam height in the white-water pit then stabilises.

When the machine speed is raised, the white-water circulation volume grows in step and the compatibility of the chemical needs to be checked together. KM-902 has excellent compatibility, producing no flocculation and no effect on paper appearance; once the three readings of temperature, size dosage and stock consistency are checked through, the fitted dosage of that paper machine is made clear and the papermaking section takes this grade as the basis for dosing during the shift.

Typical Operating Conditions and Verification

Customer case: the papermaking workshop of a paper enterprise in Jiangsu, applied to defoaming treatment of the papermaking white-water system.

At this plant the paper-surface mottling had exceeded the limit for batch after batch, the foam layer in the wire-pit white water covered more than half the pit surface, and the papermaking speed had long run below the design value. The plant selected KM-902 as the defoaming grade for that machine, with the dosage rated by white-water temperature and stock consistency. After the switch, the count of paper-surface mottling fell back within the pass range; the foam layer in the white-water pit thinned noticeably; the papermaking speed returned near the design value; and the spray piping no longer suffered flow interruption caused by foam.

Frequently Asked Questions

When the KM-902 series is used in papermaking white water, will it affect paper appearance while eliminating mechanical foam?

Depending on the share of mechanical foam in the white water, the fitted dosage of KM-902 needs to be checked together with the rosin-size dosage. This grade is a silicone-based formulation, designed for production lines where mechanical foam dominates and temperature is not the main contradiction; it does not aggravate fibre flocculation. The measured data on the count of paper-surface mottling and the foam height are given by Chemi Tech from two grades of papermaking records of the same machine, and within the rated dosage grade they do not affect paper appearance. The actual dosage is corrected by white-water temperature and stock consistency; Chemi Tech checks the records of the same machine together and gives the corresponding grade.