Elevation shot of coated metal wall panels

On a roll-coating line, an aluminium colour coil passes through its primer and top coat; before the wet film reaches the curing oven it has no time to level out, orange peel and roller marks set in during the cooling section, and a whole coil has to be downgraded.

Chemi Tech supplies levelling agents for the roll-coating systems of aluminium coils and pre-painted steel, drawn from the levelling agent KMP-4600 series; the dosage is set flexibly by application viscosity and line speed. KMP-4600 is a water-based levelling agent that lowers the dynamic surface tension, widening the levelling window of the coil line. From measured data on orange-peel grade and gloss reading, Chemi Tech grades the fitted dosage for the KMP-4600 series.

Advantages of Chemi Tech Levelling Agents

Chemi Tech levelling agent KMP-4600 series is configured for aluminium-coil roll coating and coil coating. It lowers surface tension markedly, so the wet film completes its spreading before curing and the orange peel on the panel narrows; the dynamic surface tension is held down, so no roller marks appear at high line speed; compatibility is excellent, so it pairs with water-based polyester and water-based acrylic systems without clouding the coating; intercoat adhesion is reliable, with no craters between primer and top coat; thermal stability is good, with no decomposition or yellowing across the stoving-section temperature range; and the dosage is economical, graded by application viscosity, so the number of downgraded coils falls.

Industry Pain Points and Solutions

The orange-peel problem on roll-coated panels mostly has its root in a mismatch between coating viscosity and line speed, while the curing section's too-rapid temperature rise compresses the levelling time, and it finally concentrates in two places: orange-peel grade and gloss uniformity.

Once line speed is raised, the stripes drawn out by the coating roll have no time to level, and rows of transverse marks are left on the panel. KMP-4600 lowers surface tension markedly, so the wet film completes its spreading before entering the oven.

If the temperature in the early curing oven rises too fast, the surface of the wet film skins over first, and as water and solvent escape from inside they push out pinholes. KMP-4600 widens the levelling window, so spreading completes before the surface skins over.

A downgraded aluminium coil ships at a reject price, and a single downgrade wipes out the profit of the whole coil. Grading the dosage by application viscosity and line speed keeps additive spending inside a calculable range, and the number of reworked coils on the roll-coating line narrows with it.

Typical Operating Conditions and Verification

Customer case: an aluminium-processing enterprise in Guangdong, applied to the roll-coating line for colour-coated aluminium coils.

An earlier round of viscosity adjustment did little for the orange peel, and once summer came, roller marks and gloss variation appeared together. The line's levelling agent was set to KMP-4600, with the dosage graded by application viscosity and line speed. After the switch, the panel showed: orange-peel grade down by one level; gloss readings converging to uniformity; and the pull-off test for intercoat adhesion back within acceptance limits.

Frequently Asked Questions

With a levelling agent added to the top coat, will intercoat adhesion between primer and top coat be affected?

Work out how much the roll-coating speed and the curing-section temperature rise each change, then decide which dosage grade to use. KMP-4600 has completed comparative measured tests of orange-peel grade and gloss reading in the water-based polyester and water-based acrylic systems of aluminium-coil roll coating; within the recommended range intercoat adhesion stays stable and no edge marks appear at the recoat interface. In practice the dosage is based on application viscosity, with line speed and curing curve as correction terms; Chemi Tech verifies by comparing orange-peel readings against adhesion strength, and sets the fitted dosage.