Benchtop viscometer with its matching measuring cylinder in close-up
Waterborne carbon-black paste runs a third pass in the sand mill, the grind-gauge reading stops in place and will not drop further, yet the paste viscosity climbs steadily with grinding time; after standing overnight the batch re-coagulates, and blackness and colour development both read low on the inspection sheet.
Chemi Tech supplies the KMK-216 series of dispersants for waterborne carbon-black paste and black-coating systems; the dosage is set by balancing the carbon-black specific surface area against the paste solids content. KMK-216 is a waterborne dispersant; its anchoring groups grip the carbon-black agglomerate surface and do not desorb under high-shear grinding. With the sand-mill current and grind-gauge readings placed together, the fitted dosage of the KMK-216 series answers for itself.
Advantages of Chemi Tech Dispersants
The Chemi Tech KMK-216 series dispersant is configured for the grinding and let-down stages of waterborne carbon-black paste. It grips the carbon-black surface through anchoring groups and does not desorb under high-shear grinding; the viscosity-reduction effect is marked, bringing the viscosity within a pumpable range at the same solids content; blackness rises markedly, the blackness reading sits one grade higher at the same formula; dispersibility is good, so even high-specific-surface-area carbon black is wetted fully; the colour paste is storage-stable, with no reflocculation and no flooding; and the dosage is economical, graded by carbon-black specific surface area, so the re-grind batches shrink.
Industry Pain Points and Solutions
The grinding problem of waterborne carbon-black paste has its root mostly in the combined action of carbon-black agglomerates not being fully opened and the dispersant desorbing under high shear, while the fine primary particles re-agglomerate, finally concentrating in two places: fineness no longer dropping and viscosity climbing.
High-specific-surface-area carbon black has high surface energy; when wetting is incomplete the agglomerates are crushed by the zirconium beads over and over without breaking apart. KMK-216 grips the carbon-black surface through anchoring groups without desorbing, and the agglomerates are stripped open step by step inside the grinding chamber.
As grinding time lengthens, paste viscosity climbs with the growth of fine particles, and the sand-mill current rises. Balancing the carbon-black specific surface area against the zirconium-bead size, the KMK-216 dosage lands in a suitable grade, and the current and discharge temperature stay within a controllable range.
After standing overnight the fine particles re-agglomerate, and the next morning's start-up must first run a re-grind pass. With the dosage graded by carbon-black specific surface area, the re-grind batches fall, saving both machine hours and labour.
Typical Operating Conditions and Verification
Customer case: a colour-paste enterprise in Zhejiang, applied to the grinding and let-down stage of waterborne carbon-black paste.
After the third sand-mill pass the grind-gauge reading stopped and would not drop further, while the discharge viscosity climbed steadily in the property record; re-measured after standing overnight, the paste had reflocculated and the blackness reading was one grade below target, with a re-grind pass required every next morning. Comparing the carbon-black specific surface area against the zirconium-bead size, KMK-216 was chosen for the plant, the dose taken in separate grades by paste solids content. After it went in, the agglomerates were stripped open step by step inside the grinding chamber; at the same solids content the viscosity fell into the pumpable range; the blackness reading rose one grade, and the batches lost to standing reflocculation and re-grind came down.
Frequently Asked Questions
With dispersant added to carbon-black paste, will blackness and storage stability pull against each other?
The two items placed side by side are the anchor strength and the viscosity-reduction magnitude. KMK-216 has completed comparative measured tests of sand-mill current and grind-gauge fineness in waterborne carbon-black paste; within the recommended range both items pass at once, and the paste does not reflocculate or flood after standing. With carbon-black specific surface area as the baseline and solids content and zirconium-bead size as correction terms, the dosage is settled by the comparative verification of blackness reading and storage stability.