Coloured metal sheets stacked in layers in a storage yard

After waterborne automotive paint finishes spraying, orange peel first surfaces on the basecoat panel and pinhole-like craters then appear in the clearcoat; the interlayer adhesion of the two-pass spray fails the cross-cut test inconsistently, and rework and touch-up spraying pin the throughput down at the coating step.

Chemi Tech introduces the KMP-4500 series of levelling agents for basecoat and clearcoat spray lines of waterborne automotive paint; the dosage can be adjusted flexibly with spraying tempo, wet-film thickness and flash-off window. This grade markedly lowers the dynamic surface tension, so the wet film spreads fully within the flash-off window; its compatibility is excellent and it causes no craters, while leaving margin at the recoat interface. The measured records of panel orange-peel grade and cross-cut interlayer-adhesion results are filed into the same test-panel record, and the precise dosage of the KMP-4500 series is settled at that grade.

Advantages of Chemi Tech Levelling Agents

The Chemi Tech KMP-4500 series levelling agent is configured for basecoat and clearcoat spray lines of waterborne automotive paint. It lowers the dynamic surface tension and lets the wet film spread fully within the flash-off window; edge retraction at panel edges basically does not appear and corner coverage is uniform; the panel orange-peel grade rises and gloss uniformity improves in step; its compatibility is excellent and it causes no craters; it leaves margin at the recoat interface; and its thermal stability is strong, with no decomposition or yellowing in the baking section, so the distinctness of image of the clearcoat is not disturbed.

Industry Pain Points and Solutions

The root of orange peel and craters on a spray line lies mostly in the combined effect of a too-short flash-off window and too-steep a surface-tension gradient across the wet film, while raising the chain speed further compresses the spreading time, finally concentrating in two problems: orange peel on the panel surface and interlayer adhesion.

When the spraying tempo is quickened, the wet film has no time to spread and the orange peel sets with it. KMP-4500 markedly lowers the dynamic surface tension; once spraying tempo and flash-off temperature are set, its dosage is re-rated by the chain speed of that line, and the panel orange-peel grade rises one notch.

When the wet-film thickness is set thicker, the surface-tension gradient at the panel edge amplifies and edge retraction follows. KMP-4500 performs stably across both thick-film and thin-film grades; once two paired sets of readings, wet-film thickness against baking curve and panel orange-peel grade against clearcoat crater count, are checked side by side, the addition is graded at once and edge retraction at the panel edges basically no longer appears.

After the baking curve is changed, the most easily disturbed is the recoat interface, and adhesion between clearcoat layers fluctuates with it. The KMP-4500 series leaves margin at the recoat interface and adds no extra sanding step on this item; once spraying tempo, wet-film thickness and flash-off window are set, which grade the line falls into is settled, and the coating section schedules the shift plan accordingly.

Typical Operating Conditions and Verification

Customer case: the waterborne automotive paint spray line of an automotive coating supplier in Guangdong, applied to the basecoat and clearcoat spraying and baking stages.

At this plant edge retraction at the panel edges was not obvious, yet orange peel recurred on the same panel surface and the clearcoat crater count stayed high after baking. The line switched to KMP-4500, with the addition rated by spraying tempo and wet-film thickness; panel orange-peel grade and clearcoat crater count were recorded batch by batch, and wet-film thickness against baking curve formed a separate paired comparison. Measured performance after the switch: the panel orange-peel grade rose one notch; edge retraction at the panel edges basically no longer appeared; and the cross-cut result of interlayer adhesion for the two-pass spray passed stably.

Frequently Asked Questions

If the levelling-agent dosage is increased, will it instead cause craters or weaken interlayer adhesion?

The panel orange-peel grade and the cross-cut interlayer-adhesion result must be checked side by side. The KMP-4500 series has excellent compatibility and causes no craters at normal dosage; the measured data of orange-peel grade and gloss readings are checked out by Chemi Tech from the test-panel records of the same spray line, and within the above comparison range they do not weaken interlayer adhesion. The addition is re-calibrated by spraying tempo and wet-film thickness; once the test-panel records and production-line readings are checked together, Chemi Tech fixes the precise dosage of that line.