Circular sedimentation tanks and rectangular tank bodies of a wastewater treatment plant arranged in groups from above

After the mixing-water ratio of the dry-mix mortar mixer is raised, the air entrained is slow to escape, the compactness of the moulded test blocks declines accordingly, the setting time of the gypsum system is pulled out of tolerance, and hollowing and cracking of the plastered surface concentrate on this batch.

Chemi Tech has introduced the KM-955 series of defoamers for dry-mix mortar and gypsum systems; the dosage is adjusted flexibly by mixing-water ratio and gypsum content. This grade is a powder formulation; it breaks foam rapidly on contact with water and does not change the intended action of retarders and water reducers. The measured data on the air content of the fresh mix and the compactness readings of the test blocks are brought together for checking, and the precise dosage of the KM-955 series is read from them; Chemi Tech assigns the dosage grades to each batch according to the differences in powder grading and gypsum grade from plant to plant.

Advantages of Chemi Tech Defoamers

The Chemi Tech KM-955 series defoamer is configured for dry-mix mortar and gypsum systems. Its defoaming speed is fast, and the air entrained in the fresh mix inside the mixing drum is discharged rapidly; its stability is strong, and the foam-suppressing capacity does not decay in the alkaline environment of the gypsum system; its compatibility is excellent, and it does not change the intended action of retarders and water reducers; and its foam-suppressing duration is long-lasting, so no replenishment is needed within the gypsum setting window, and the air-content reading of each batch of dry mix is kept batch by batch in the mixing records.

Industry Pain Points and Solutions

The root of high air content in dry-mix systems lies mostly in the combined effect of a raised mixing-water ratio and a too-fine powder grading, while a higher gypsum content compresses the setting window to a critical point, finally concentrating in two places: the compactness of the test blocks and hollowing of the plastered surface.

When the mixing-water ratio is raised, the micro-bubbles in the fresh mix are wrapped in a water film, the compactness after the test blocks are moulded drops first, and hollowing of the plastered surface increases in step. KM-955 breaks foam fast; once the two readings of mixing-water ratio and fresh-mix air content are set, its fitted dosage is re-rated by the charge weight of each batch, and the compactness reading returns near the design grade.

After the gypsum content is turned up, the setting window narrows, micro-bubbles are fixed in the test blocks before they can escape, and the two sets of readings, compactness and setting time, deviate together. The KM-955 series has strong stability; once the compactness and setting-time readings of the same batch before and after the content adjustment are compared side by side, the dosage is rated at once to the fitted grade of that formulation, the setting time returns to the middle of the interval, and the compactness no longer fluctuates with the content.

When the powder fineness is narrowed, the specific surface area grows and the difficulty of dispersing a powder defoamer rises one notch. The KM-955 series disperses well as a powder and adds no extra pre-mixing cycles on this item; once the three readings of water ratio, content and fineness are checked through, the precise dosage of that formulation is made clear, and the mixing plant fixes the charge weight of each batch accordingly.

Typical Operating Conditions and Verification

Customer case: the dry-mix workshop of a ready-mixed mortar producer in Hebei, applied to the batching and mixing stages of gypsum-based plastering mortar.

After this plant switched to a batch of powder with a narrower fineness for its gypsum-based plastering mortar, the compactness reading of the test blocks fell from the pass grade to its lower edge, the rework volume for hollowing of the plastered surface rose batch by batch, and the setting time swung nearly a quarter of an hour around the set value. KM-955 was selected as the defoaming grade for this dry-mix line, with the addition rated by mixing-water ratio and gypsum content. After commissioning, the air content of the fresh mix fell from nine percentage points to around four percentage points, and the compactness reading of the test blocks returned from the lower edge to the design grade; the two sets of readings were given side by side in the same mixing record, and the deviation of the setting time was brought into the set interval.

Frequently Asked Questions

Will the KM-955 series powder defoamer throw the action of the retarder off course in dry mix?

What are compared together are the three sets of readings: fresh-mix air content, test-block compactness and setting time. The KM-955 series is a powder formulation and breaks foam rapidly on contact with water; the measured data of these three sets of readings are checked out together by Chemi Tech from the controlled records of the same formulation, and within the rated dosage grades it does not change the intended action of retarders and water reducers. The on-site charge is weighed separately by the mixing-water ratio and powder fineness of each batch; Chemi Tech determines the precise dosage of that formulation from bench tests and mixing records.