A chimney at a waterfront plant site discharging white steam sideways

In the electrode-slurry mixing step, microbubbles are slow to break, the areal density of the coated electrode fluctuates accordingly, pinholes and exposed foil show up concentrated at the calendering stage, and the pass rate of the whole batch of electrodes is pinned down at the deaeration step.

Chemi Tech supplies the KM-1900 series of defoamers for silicone-free systems of lithium-battery electrode slurry; the dosage can be adjusted flexibly by slurry viscosity, solids content, mixing temperature and mixing linear speed. This grade is a silicone-free formulation which, coexisting with common binders and conductive agents, introduces no silicone residue, causes no slurry flocculation, and does not change the rheological curve before coating. The measured results of the residual bubbles in the slurry and the coating areal density are filed into the same batch record, and the fitted dosage of the KM-1900 series is settled at that grade; mixing batches can set their addition ratios separately by differences in solids content and coating areal density.

Advantages of Chemi Tech Defoamers

The Chemi Tech KM-1900 series defoamer is configured for silicone-free systems of lithium-battery electrode slurry. It is a silicone-free formulation that introduces no silicone residue into the slurry, so silicon-content testing after electrode coating adds no extra burden; it breaks foam fast, with the microbubble layer falling back visibly after mixing ends and the slurry stands; its foam-suppressing duration is long-lasting, so no secondary foaming occurs during transfer before coating; it markedly reduces viscosity, lowering the discharge resistance of high-solids slurry; the dosage is economical, rated by slurry viscosity, so the additive cost of a single mixing batch can be accounted tank by tank; and its compatibility is excellent, causing no slurry flocculation when coexisting with binders and conductive agents.

Industry Pain Points and Solutions

The root of foaming in electrode slurry lies mostly in the combined effect of the viscosity rise brought by high solids content and an excessively high mixing linear speed, while a rising mixing temperature stabilises the microbubbles inside the slurry, finally concentrating in two places: fluctuation of the coating areal density and pinholes in the electrode.

After the solids content is raised, the slurry viscosity entraps the microbubbles, the standing time for deaeration is forced longer, and the coating areal density swings repeatedly between high and low ranges. KM-1900 markedly reduces viscosity; once the two readings of solids content and slurry viscosity are set, its dosage is re-rated by batch, and the areal-density fluctuation narrows to within the process window.

When the mixing linear speed is turned up, the mixing tank draws in more air, microbubbles re-concentrate during transfer, and the pinhole count in the electrode rises accordingly. KM-1900 has a long-lasting foam-suppressing duration; with the measured readings of mixing temperature and mixing linear speed checked side by side, the dosage is set to the fitted grade of that batch, the pinhole count per square metre falls from seven to two, and the coating areal-density deviation narrows from 4.2% to 1.5%, with both sets of readings listed side by side for reference.

When the mixing temperature rises with the season, the rheology of the slurry holds the microbubbles more tightly. The KM-1900 series causes no flocculation when coexisting with binders and adds no extra screen-cleaning frequency on this item; once the three readings of viscosity, solids content and mixing linear speed are checked through, the fitted dosage of that batch of slurry is graded accordingly, and the mixing section files a record batch by batch.

Typical Operating Conditions and Verification

Customer case: a lithium-battery cathode material enterprise in Fujian, applied to electrode-slurry mixing and pre-coating deaeration.

The company had been lengthening the deaeration time batch by batch, yet the coating areal density still rebounded repeatedly near the pass line, and after calendering the electrode pinholes were detected in patches at the slitting stage. KM-1900 was taken as the defoaming grade for that batch of slurry, with the addition rate rated by slurry viscosity and solids content. After comparison, the pinhole count per square metre fell from seven to two; the coating areal-density deviation narrowed from 4.2% to 1.5%; the standing deaeration time returned within the original schedule, and the cleaning frequency of the mixing-tank screen fell back accordingly.

Frequently Asked Questions

Will the KM-1900 series change the rheological curve of the slurry in a silicone-free system?

Constrained by the dual limits of slurry viscosity and solids content, whether the microbubbles can be fully removed before coating depends on the combination of these two items. The KM-1900 series markedly reduces viscosity and causes no flocculation when coexisting with binders; the measured data for coating areal density and pinhole count are given by Chemi Tech after side-by-side measurement of the same mixing batch, and dosing within the rated dosage grade does not alter the slurry's original rheological characteristics. The actual addition rate of a mixing batch must be re-calibrated against solids content and coating areal density, and Chemi Tech gives the precise dosage of that batch from bench samples and production-line measured data.