Red-brick plant buildings meeting a tall, slender chimney under a pale sky

Once the circulating slurry of a wet desulfurization tower foams, the slurry density reading at the absorber tower runs falsely high, the demister differential pressure rises in step, and the droplet carryover in the clean flue gas and the cavitation of the gypsum discharge pump appear together.

Chemi Tech supplies the KM-1446 series of defoamers for the slurry recirculation conditions of wet flue gas desulfurization; the dosage is adjusted flexibly by the slurry density and the slurry pH value. This grade resists acid and shear, does not decompose or fail in the high-salinity slurry of the absorber tower, and does not change the particle-size distribution of the gypsum crystals. The two sets of readings, the foam-layer height in the absorber tower and the demister differential pressure, are laid out on the same operating record, and the precise dosage of the KM-1446 series is settled at that grade of the tower.

Advantages of Chemi Tech Defoamers

The Chemi Tech KM-1446 series defoamer is configured for slurry recirculation in wet flue gas desulfurization. It resists acid and shear, and its foam-suppressing ability does not decay under high-salinity slurry and high-speed circulation pumps; it does not affect gypsum crystallisation, and the moisture content of the dewatered gypsum stays stable; it breaks foam fast, and the foam-layer height in the absorber tower drops markedly; it forms no scale on the demister, and the flushing cycle is not shortened by dosing; and the defoaming cost per tonne of slurry is rated by switching on slurry density and pH value, so it can be accounted for each unit.

Industry Pain Points and Solutions

The root of foaming in the desulfurization-tower slurry lies mostly in the combined effect of a high slurry density and the shear of the oxidation air, while the falling slurry pH value further stabilises the fine bubbles inside the tower, finally concentrating in two places: the foam layer in the absorber tower and the demister differential pressure.

When the slurry density runs high, the foam in the absorber tower first covers the whole surface and the falsely high slurry density reading follows. KM-1446 resists acid and shear; once the two readings of density and liquid-to-gas ratio are cleared, its dosage is re-rated by the load inside the tower and the foam-layer height falls back.

After the slurry pH value falls, fine bubbles are entrained into the slurry by the oxidation air and the demister differential pressure rises in step. KM-1446 breaks foam fast; with the cavitation reading of the gypsum discharge pump and the demister differential pressure laid out on the same record sheet, the dosage is graded as soon as the two sets of readings are cross-checked side by side, and the differential pressure no longer climbs shift by shift.

The particle size of the gypsum crystals must likewise be checked together. The KM-1446 series does not affect gypsum crystallisation and adds no extra dewatering-machine adjustment on this item; once the three items of density, pH value and liquid-to-gas ratio are checked through, the precise dosage of that tower is settled and the desulfurization operating crew executes accordingly.

Typical Operating Conditions and Verification

Customer case: the wet desulfurization operating workshop of a thermal power generation enterprise in Jiangsu, applied to foam control at the absorber-tower slurry recirculation and the demister.

At this power company the desulfurization-tower slurry density reading had long been inconsistent with field sampling, the set value of the demister differential pressure had to be raised once every shift, and the droplet carryover in the clean flue gas repeatedly crossed the line in on-line monitoring. KM-1446 was selected for the plant, with the dosage rated by slurry density and pH value. Measured performance after the switch: the slurry density reading came into line with the sampling result; the demister differential pressure no longer climbed shift by shift; the moisture content of the dewatered gypsum returned to near the design value, and the current fluctuation of the oxidation blower narrowed in step.

Frequently Asked Questions

When a defoamer is used in the desulfurization slurry, will the demister differential pressure keep climbing?

What directly decides the trend of the differential pressure is the dissipation speed of the foam layer inside the tower. The KM-1446 series resists acid and shear and forms no scale on the demister; the measured data on foam-layer height and demister differential pressure are given by Chemi Tech after side-by-side comparison of the same absorber tower, and dosing at the rated magnitude does not change the original pace of gypsum crystallisation. The actual dosage is referenced to slurry density and pH value; Chemi Tech brings the two sets of differential-pressure readings together to work out the fitted dosage.