Colored powders in a multi-compartment round dish arranged in groups seen from above
After a batch of filler grades was changed for an epoxy floor coating color match, the fineness reading of the mill base refused to come down, floating and flooding showed up together in the rub-out test, and the same formulation had to be readjusted with every new filler batch, pinning the delivery schedule down at the color-matching step.
For the pigment-and-filler dispersion system of epoxy floor coatings, Chemi Tech supplies the KMK-409 series of dispersants; the dosage is adjusted flexibly by filler grade, surface-treatment method, target solids content and milling time. This grade uses anchoring groups to grip the filler surface and does not desorb under high-shear milling; it reduces viscosity markedly and adapts widely to both inorganic and organic pigments and fillers. The fineness reading of the mill base and the rub-out floating rating are listed separately by grade, and the precise dosage of the KMK-409 series can be read out grade by grade.
Advantages of Chemi Tech Dispersants
The Chemi Tech KMK-409 series dispersant is configured for the pigment-and-filler dispersion of epoxy floor coatings. Its anchoring groups grip the filler surface and do not desorb under high-shear milling; it reduces viscosity markedly and the sand mill current stays steady and controllable; it adapts widely to both inorganic and organic pigments and fillers, so changing grades does not require a full readjustment; its storage stability is strong and the mill base neither coarsens nor floats; its tinting strength and color development stay stable and the rub-out floating rating remains consistent; and the dosage is switched by filler grade and target solids content, so the additive cost of the color-matching workshop can be accounted color family by color family.
Industry Pain Points and Solutions
The root of floating and flooding in a floor-coating system lies mostly in the mismatch between the surface treatment of the filler and the anchoring groups of the dispersant, while a higher target solids content compresses the distance between particles to a critical value, finally concentrating in two places: fineness rebound and rub-out flooding.
As soon as the filler grade changes, the previously attached dispersant is pulled off course by the polarity of the new surface and the fineness reading rebounds around the acceptance line again and again. KMK-409 performs attachment comparison by filler grade and surface-treatment method; once the two clues are cleared, the dosage is rated grade by grade, and the fineness reading stops rebounding.
Once the target solids content is raised, the mill-base viscosity pushes up the sand mill current, the milling time is forced longer, yet the fineness still will not come down. KMK-409 reduces viscosity markedly; with the two sets of readings compared side by side, the target solids content rises from 45% to 52%, the sand mill current falls from 32 amperes to 26, and the mill-base fineness converges in step.
Coarsening and floating during storage are also within consideration. The KMK-409 series anchors fully and adds no extra re-milling passes on this item; once the four comparisons of grade, surface treatment, solids content and milling time are complete, the precise dosage of that color family can be graded and the color-matching workshop doses by grade.
Typical Operating Conditions and Verification
Customer case: the color-matching workshop of a floor-coating enterprise in Guangdong, applied to the milling and blending stages of epoxy floor coating pigments and fillers.
That plant changed three filler suppliers in the first half of the year; the fineness readings of the same formulation differed noticeably across the three grades, and the rub-out floating rating passed on only one of the grades. KMK-409 was selected as the general-purpose grade for that color-matching workshop, with the dosage graded by filler grade and target solids content. After the comparison: the fineness readings of the three grades converged; the floating ratings all fell inside the acceptance range; the sand mill current no longer swung widely with the grade, and the number of re-milling passes decreased.
Frequently Asked Questions
Can one dispersant handle several filler grades at once?
The two clues of filler surface treatment and target solids content must be checked together. The KMK-409 series makes filler-by-filler attachment comparisons by filler grade and adapts widely to both inorganic and organic pigments and fillers; the fineness reading and the rub-out floating rating are given by Chemi Tech from filler-by-filler comparisons of the same color family, and within the rated dosage range they do not weaken tinting strength. The actual dosage is corrected by filler grade and target solids content; Chemi Tech gives the dosage of that color family from the filler-by-filler comparison results.